Thermo-Mechanical Properties of Synthetic Fibres Filled with Ceramic Filler Reinforced Epoxy Hybrid Composites

This study evaluates the thermo-mechanical features of hybrid epoxy composites reinforced with carbon, E-glass, and S-glass fibres, incorporating 10 wt % alumina (Al₂O₃) filler. Laminates were fabricated via hand lay-up using 45 wt % fibre and 45 μm alumina particles. EDAX and SEM confirmed high-purity alumina with sub-angular morphology. Thermo-mechanical properties were studied using DSC, TGA, and DMA techniques. DSC showed S-Ec/Al₂O₃ 10 had the highest peak temperature (396.68 °C), indicating strong thermal transition stability. C-Ec/Al₂O₃ 10 showed the highest heat absorption (46.97 J/g), indicating greater enthalpic response. TGA revealed all composites decomposed near 880 °C, with C-Ec/Al₂O₃ 10 retaining the most residual mass (47.06 %). S-Ec/Al₂O₃ 10 had the lowest residual mass (21.16 %), indicating rapid post-transition breakdown. DMA results showed C-Ec/Al₂O₃ 10 had the highest storage (12941.70 MPa) and loss modulus (2199.94 MPa). It also had the highest damping factor (Tan δ = 0.575), indicating superior mechanical damping. E-Ec/Al₂O₃10 recorded the highest thermal onset (152.42 °C), showing strong thermal stiffness retention. C-Ec is ideal for high-strength damping use, E-Ec for thermal endurance, and S-Ec for moderate load applications. Major Findings: C-Ec/Al₂O₃10 showed the highest heat absorption, residual mass, and mechanical properties, indicating superior thermal resistance and stiffness. S-Ec/Al₂O₃ 10 had the highest DSC peak but degraded fastest, while E-Ec/Al₂O₃ 10 had the highest onset temperature; fillers were pure and well-bonded.

View article page

Download PDF