This article presents a physical and chemical investigation of Silicone insulating Rubber (SiR) composite insulators. The study employs durometer shore A measurements, Thermogravimetric Analysis (TGA), and ATR with Fourier Transform Infrared Spectroscopy (FTIR) to evaluate various types of SiR, including 420 kN/800 kV, 210 kN/500 kV, 160 kN/400 kV, 120 kN/400 kV, 90 kN/66 kV, 70 kN/220 kV, 45 kN/25 kV, to assess their performance as insulators for power sector applications. The TGA, conducted according to ASTM E1131, provides a detailed thermal decomposition analysis of SiR and determines filler content and characteristic values unique to the material. Similarly, FT-IR analysis, performed as per ASTM E1252, identifies specific chemical groups and characteristic bands of the material. SiR is primarily composed of polydimethylsiloxane (PDMS) and is enhanced with inorganic fillers such as Alumina Trihydrate (ATH) for High-Temperature Vulcanized (HTV) applications. The TGA study indicates that thermal decomposition occurs in two key stages: the release of highly volatile organics and the breakdown of organic components within the silicone polymer. Notable findings from the FT-IR analysis confirm the presence of PDMS and the hydroxyl (OH) group of ATH in SiR. The hardness of SiR is measured using the IEC 62217 method. Results indicate that the silicone content of SiR ranges from 31% to 37% according to TGA, and hardness values increase from 68 to 71 due to the aging process. Remarkably, a maximum increase of 4 in hardness was observed after aging. This research emphasizes the strength and reliability of SiR composite in demanding power sector applications.