Corrosion Studies of a Few Aluminium, Copper, Nickel and Iron Base Alloys in Salt Water

A few alum inium , copper, nickcl and iron base alloys have been subjected to corrosion tests up to 15 days in 3% NaCI solution and synthetic sea water under various conditions o f experim ent. A nodic polarisation studies reveal that there is no passivity but dissolution and the general pattern o f the cathodic polarisation curve* is observed to be the sam e for all the conditions o f experim ents studied. There is slight pitting observed for alum inium alloys while copper, nickcl and iron base alloys do not exhibit pitting tendency. Alum inium brass, nick el-free austenitic stainless steel and Hastelloy X merit consideration for use in salt water service.