Ellipsometric and Cyclic Voltammetric studies of Corrosion of Carbon Steel in K2S 04 Solution in presence of NaN02
CORROSION behaviour of carbon stool and the characteristics of tho film formed on its surface inlC.SO,, NaNO* and K.jS0 4 -fN aN O j solutions were studied by direct weight loss, cyclic voltam m etry and ellipsom etry. Direct w eight loss measurements havo shown corrosion inhibition efficiency of ~ 99% in 200 ppm NaNO.. solution and about 88% in a solution containing a m ixture of 800 ppm N aN O ยป and 400 ppm K tSO t . Cyclic voltam m etry was carried out between-1600 mV and + 800 mV (vs. SCE) in 400 ppm K .S O ,, 800 ppm NaNO, and 400 ppm K.SO , + 800 ppm N aNO j solutions. The steel dissolved freely in K ,S O ,. In NqNO., and K .S O , + NeNO > solutions, tho voltam m etric behaviour was sim ilar. Three peaks appeared on the anodic cycle w hile tw o on the cathodic cycle. Tho voltam - mogram showed high degree of polarization. From ellipsom etric measurements in 100 and 200 ppm N aN O ,, the film refractive index was found to be 1.69 (1 -0 .Oi). 3 0 The film thicknesses were 29.0 A and 25.5 A after 4 hours of exposure. In case of K-jSOt + NaNO,* solutions the film was found to have the refractive index of 1.63 (1-0.03*) w ith a thickness of 71.8 A in 24 hours. The results suggost that in presence of N aN O ;, corrosion of m ild stool In K ;S 0 4 solution is inhibited by the form ation of passivo FoO(OH) layer