Electrochemical Characterization Of CaCl2-48 MOL % NaCl (0-2 % wt.% CaO) Melts And Study Of The Electrochemical Behavior Of Platinum As Anode In The Melt System
Electrochemicalinvestigationswere carriedoutonCaCl2 -48mol.%NaCl(0-2wt.%CaO)melts at650 oC, as part of a study to select an electrolytemelt containingCaCl2 for direct electro-reduction ofsolid UO2 to U metal. Decomposition potentials ofCaCl2 -48mol.%NaClmeltwasmeasuredusing linear polarizationmethodand found to be 3.33 V.Cyclic voltammetry oftungsten, graphite and platinum working electrodes against aNi/NiO reference electrodewas carried out with and without addition of CaO in themelt. In pureCaCl2 -48mol.% NaCl melt, the cathodic Na-Ca alloy formation on tungsten (2Na+ -Ca2+ + 2e- ‹ Na-Ca) occurred at -2.26 V and the anodic chlorine gas evolution on graphite (2Cl- ‹ Cl2 + 2e- ) at +1.09 V. The anodic reaction on platinum, consideredpredominantlyduetochlorinegas evolution andinasmallmeasuretoplatinumdissolution,Pt‹ Pt2+ + 2e- ,wasfoundto occur at +1.02V in the same melt. In CaCl2 -48mol% NaCl-(1-2) wt.%CaOmelts, the onset of oxygen evolution on Pt working electrode (2O2- ‹ O2 + 2e- ) occurred at + 0.65V and chlorine gas evolution at +1.04V.The resultsindicated the possibility ofusing Pt as an anodewithminimumconsumption in the electro- reduction ofUO2 inCaCl2 -48 mol% NaCl-(1-2) wt.%CaOmelt.The reaction, 2O2- ‹ O2 + 2ewasfound to be diffusioncontrolled inthe range ofscanrates,1-5V/sandthediffusioncoefficientofO2- ionswas calculated to be 9.9 x 10-6 cm2 s -1 at 650 oC.