Microstructural Characterization Of Plasma Sprayed LaPO<sub>4</sub> Based Coating

Deposition of lanthanum phosphate coating was carried out using 80 kW atmospheric plasma spray system. Spherical powder for the same, in the size range 22-45 ìm, was obtained by spray drying. The thickness of the coating was controlled in the range of 275-325 ìm in order to have sufficient adhesion strength. The compatibility of LaPO4 towards plasma spraying and its parameter such as plasma forming gas flow rate have been studied using microstructural characterization. High gas flow rate was found to be favorable for synthesizing quality coating with which high amount of porosity can be tailored leading to further decrease in thermal conductivity of the coatings. X-Ray Diffraction and FESEM study revealed the presence of LaPO4 and the formation of a secondary phase i.e. La2O3 which is further confirmed by Micro-Raman spectroscopy. The formation of La2O3 phase can be reduced to some extent by controlling the rate of flow of plasma forming gas.