Stress Corrosion Cracking Resistance of Type 316L(N) Stainless Steel Weld Joints

Stress corrosion cracking resistance (SCC) of AISI type 316L(N) stainless steel weld joints fabricated using conventional TIG and Activated-TIG (A-TIG) welding processes are evaluated and compared with the 316L(N) base metal. Delta ferrite (ä ferrite) measurements and tensile tests were carried out for TIG and ATIG weld joints. SCC tests were carried out using a constant load testing technique at 60% yield strength (YS) of the material. Testing environment was concentrated solution of sodium chloride acidified using hydrochloric acid. SCC results indicated superior resistance of 316L (N) base metal compared to TIG and ATIG welds. Inferior corrosion resistance of welds is attributed to the presence of δ ferrite in the welds. ferrite results in increased microstructural and microchemical heterogeneities in weld metal as compared to a base metal. Among the weld joints, A-TIG exhibited higher resistance to SCC than the TIG due to the (austenitic-ferritic) AF solidification mode, and to the resultant microstructure produced autogenously in a single pass. On the other hand, the presence of a higher amount of δ ferrite and multipass welding of TIG welds causes extensive segregation of sulphur and phosphorous at the ferrite/ γ austenite interfaces. Interfaces acts as pre-existing active paths along which corrosive attack progresses. It causes degradation in localised corrosion resistance of conventional TIG. Time to failure is high for base material (446 hrs) followed by A-TIG weld joint (306 hrs) than the TIG weld joint (232 hrs). Therefore A-TIG welding is preferable to fabricate the structural components and sodium carrying pipes in the nuclear industry than the conventional TIG welding process.

View article page

Download PDF