Investigations on the Failure of Super 304H Grade Final Reheater Tubes of 660 MW Supercritical Boiler

An investigation into multiple reheater tube failures in a 660 MW supercritical thermal power station has been conducted. In the present study, the failure of the reheater tube in the vicinity of the tube-to-spacer weld joint has been analysed in detail, involving the evaluation of mechanical, metallurgical, and microstructural degradation, among other factors, to determine the possible root cause of the failure. The failure analysis indicated that the Super 304H tube leakage is linked to sensitisation due to exposure to higher temperatures and the welding methodology followed. The failed service-exposed and virgin tube specimens were studied in the current work. The service exposed samples that exhibited failed openings at multiple locations around the weld joint, with severe wall thinning having been observed. The root cause of the failure has been identified as the sensitisation of the metal due to high concentrations of phosphorus and chromium along the grain boundaries.

View article page

Download PDF