Root Cause Analysis of SA213 T91 Superheater Tube of a Supercritical Power Plant

The premature failure of a SA213 T91 final superheater tube from an 800 MW supercritical coal-fired thermal power plant was investigated after 67,962 hours of service at high steam pressure (250 bar) and flue-gas temperatures of 800- 970°C. The tube exhibited a longitudinal rupture accompanied by localised bulging, suggesting progressive deformation before failure. Although chemical analysis confirmed compliance with ASME SA213 T91 specifications, hardness reduction and loss of tensile strength were observed near the failed region. Microstructural examination revealed degradation of the tempered martensitic structure, characterised by carbide coarsening and preferential grain-boundary precipitation. Extensive grain-boundary cavitation and intergranular fracture features confirmed advanced creep damage. The failure was attributed to localised creep-induced microstructural and strength degradation during prolonged high-temperature exposure, resulting in tube rupture.

View article page

Download PDF